We classified the paraffin wax with a melting point of 56 to 62 ℃ medium melting point paraffin wax. By oil content and the degree of refinement, the crude versions fall into the slack wax category and contain oil content of 3% to 15%. After de-oiling, desulfurization and hydrogenation refining to remove impurities and discoloration, the oil content can 0.5%-2%. We normally separate them by semi refined paraffin wax and fully reply paraffin wax. Fully refined is the highest refinement, the oil content below 0.5% (for some high melt paraffin wax, the oil content may be below 0.75%). Semi refined paraffin waxes contain between 0.5 and 1.5% oil. Below we give you the product in this category together with their preference usage. If you didn't find the grade in below list, please send us inquiry.
We supply a variety of packaging formats. These include bulk liquid (via tank truck or railcar), slabs (10 lbs), free-flowing granules (packaged in bags), and free-flowing pastilles (packaged in bags).
Fully Refined Paraffin Wax
| UNIT | KH Paraffin Wax F56H/N/L | KH Paraffin Wax F58H/N/L | KH Paraffin Wax F60H/N/L | KH Paraffin Wax F62H/N/L |
Melting Point (ASTM D87) | ℃ | 56-58(133-136℉) | 58-60 (136-140℉) | 60-62(140-144℉) | 62-64(144-147℉) |
Oil Content (ASTM D721) | % | <0.75% | <0.75% | <0.75% | <0.75% |
Color saybolt (ASTM D156) |
| 25 | 25 | 25 | 25 |
Penetration (ASTM D1321) | 0.1mm at 25℃ | <17 | <17 | <17 | <17 |
Application | Hot Melt Adhesives |
| * | * | * |
PVC lubricant |
| * | * | * | |
Package & Coating | * |
| * | * | |
Rubber Processing |
| * | * | * | |
Polish |
|
| * | * | |
Paints & Ink |
|
|
|
| |
Fertilizer |
|
| * | * | |
Personal care | * | * | * | * | |
Candles | * |
| * |
| |
woods | * |
| * |
| |
Chlorinated paraffin wax | * | * |
|
| |
Matches | * | * |
|
| |
Rust prevention |
|
|
|
| |
Texile | * | * |
|
| |
| Blending | * | * | * | * |
Semi Refined Paraffin Wax & Slack Wax
| UNIT | KH Paraffin Wax SR56 | KH Paraffin Wax SR58 | KH Paraffin Wax SL5802 | KH Paraffin Wax SL6013 | KH Paraffin Wax SL6035 | KH Paraffin Wax SL5857 |
Melting Point (ASTM D87) | ℃ | 56-58(133-136℉) | 58-60 (136-140℉) | 58-60 (136-140℉) | 60-66 (140-151℉) | 60-66 (140-151℉) | 58-70 (136-158℉) |
Oil Content (ASTM D721) | % | <1.5% | <1.5% | <2% | 1-3% | 3-5% | 5-7% |
Color saybolt (ASTM D156) |
| 23 | 23 | 5 | 1-10 | 1-10 | 1-10 |
Penetration (ASTM D1321) | 0.1mm at 25℃ | <22 | <22 | _ | _ | _ |
- |
Application | Hot Melt Adhesives |
|
|
|
|
|
|
PVC lubricant |
|
|
|
|
|
| |
Package & Coating |
|
|
|
|
|
| |
Rubber Processing |
|
|
|
|
|
| |
Polish |
|
|
|
|
|
| |
Paints & Ink |
|
|
|
|
|
| |
Fertilizer |
|
|
|
|
|
| |
Personal care |
|
|
|
|
|
| |
Candles | * | * | * |
| * |
| |
woods | * |
| * | * | * |
| |
Chlorinated paraffin wax |
|
|
|
|
|
| |
Matches | * |
|
|
|
|
| |
Rust prevention |
|
|
|
|
|
| |
Texile |
|
|
|
|
|
|
Storage
Please store products in a cool, dry location, away from sources of intense heat, incompatible materials, water, heat, and flame.
Long-distance transportation or hot atmosphere may have cracked, that does not affect the quality of products.
If you are wondering about how to melt paraffin wax,don’t hesitate to contact.